NIOSHTIC2 Publications Search Recovery of ...
This investigation showed that treatment of the slag in hydrogen prior to leaching enhanced manganese extraction. Up to 80 pct of the manganese and 50 pct of the iron could be extracted from a silicon steel slag that had been pretreated in hydrogen at 700 deg. C.